Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 22 % Show Material materials with Elongación A50 of 22 % |
Estricción | 20.0 °C | 35 % Show Material materials with Estricción of 35 % |
Resistencia a la tracción | 20.0 °C | 585 MPa Show Material materials with Resistencia a la tracción of 585 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 365 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 365 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 0.35 % Show Material materials with Cromo of 0.35 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 - 1.4 % Show Material materials with Manganeso of 1 - 1.4 % |
Molibdeno | 0.1 - 0.3 % Show Material materials with Molibdeno of 0.1 - 0.3 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Vanadio | 0.03 % Show Material materials with Vanadio of 0.03 % |
Wolframio | 0.1 % Show Material materials with Wolframio of 0.1 % |