General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Elongación A50 | 20.0 °C | 0 - 15 % Show Material materials with Elongación A50 of 0 - 15 % | |
Estricción | 20.0 °C | 0 - 30 % Show Material materials with Estricción of 0 - 30 % | |
Resistencia a la tracción | 20.0 °C | 0 - 795 MPa Show Material materials with Resistencia a la tracción of 0 - 795 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 690 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 690 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.035 % Show Material materials with Azufre of 0 - 0.035 % |
Boro | 2E-3 - 6E-3 % Show Material materials with Boro of 2E-3 - 6E-3 % |
Carbono | 0.05 - 0.2 % Show Material materials with Carbono of 0.05 - 0.2 % |
Cobre | 0 - 0.5 % Show Material materials with Cobre of 0 - 0.5 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Manganeso | 0.6 - 1 % Show Material materials with Manganeso of 0.6 - 1 % |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % |
Silicona | 0 - 0.8 % Show Material materials with Silicona of 0 - 0.8 % |
Wolframio | 0 - 0.1 % Show Material materials with Wolframio of 0 - 0.1 % |