Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.15 % Show Material materials with Azufre of 0.15 % |
Carbono | 2.8 - 3.6 % Show Material materials with Carbono of 2.8 - 3.6 % |
Cromo | 1.4 - 4 % Show Material materials with Cromo of 1.4 - 4 % |
Fósforo | 0.3 % Show Material materials with Fósforo of 0.3 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 1 % Show Material materials with Molibdeno of 1 % |
Níquel | 3.3 - 5 % Show Material materials with Níquel of 3.3 - 5 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |