General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Densidad of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell | 23.0 °C | 121 - 171 [-] Show Material materials with Dureza Brinell of 121 - 171 [-] | |
Elongación | 23.0 °C | 30 % Show Material materials with Elongación of 30 % | |
Energía de impacto Charpy | 23.0 °C | 20 J Show Material materials with Energía de impacto Charpy of 20 J | |
Límite elástico Rp 0,2 | 23.0 °C | 205 MPa Show Material materials with Límite elástico Rp 0,2 of 205 MPa | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa | Typical for Cast Iron |
Resistencia a la tracción | 23.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Calor específico of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Material materials with Conductividad térmica of 55 W/(m·K) | Typical for Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Carbono | 2.2 - 2.7 % Show Material materials with Carbono of 2.2 - 2.7 % |
Cromo | 0.2 % Show Material materials with Cromo of 0.2 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Manganeso | 3.75 - 4.5 % Show Material materials with Manganeso of 3.75 - 4.5 % |
Níquel | 21 - 24 % Show Material materials with Níquel of 21 - 24 % |
Silicona | 1.5 - 2.5 % Show Material materials with Silicona of 1.5 - 2.5 % |