General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Resistencia a la tracción | 23.0 °C | 360 MPa Show Material materials with Resistencia a la tracción of 360 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Calor específico of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Conductividad térmica of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Boro | 7E-3 % Show Material materials with Boro of 7E-3 % |
Carbono | 0.2 - 0.3 % Show Material materials with Carbono of 0.2 - 0.3 % |
Cromo | 25 - 29 % Show Material materials with Cromo of 25 - 29 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 5 - 6 % Show Material materials with Molibdeno of 5 - 6 % |
Níquel | 1.7 - 3.8 % Show Material materials with Níquel of 1.7 - 3.8 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |