Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 248 - 341 [-] Show Material materials with Dureza Brinell of 248 - 341 [-] |
Dureza Rockwell C | 23.0 °C | 24 - 37 [-] Show Material materials with Dureza Rockwell C of 24 - 37 [-] |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % |
Estricción | 23.0 °C | 18 % Show Material materials with Estricción of 18 % |
Límite elástico Rp 0,2 | 23.0 °C | 585 MPa Show Material materials with Límite elástico Rp 0,2 of 585 MPa |
Resistencia a la tracción | 23.0 °C | 895 MPa Show Material materials with Resistencia a la tracción of 895 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.28 - 0.35 % Show Material materials with Carbono of 0.28 - 0.35 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 18 - 21 % Show Material materials with Cromo of 18 - 21 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.75 - 1.5 % Show Material materials with Manganeso of 0.75 - 1.5 % |
Molibdeno | 1 - 1.75 % Show Material materials with Molibdeno of 1 - 1.75 % |
Niobio | 0.25 - 0.6 % Show Material materials with Niobio of 0.25 - 0.6 % |
Níquel | 8 - 11 % Show Material materials with Níquel of 8 - 11 % |
Silicona | 0.3 - 0.8 % Show Material materials with Silicona of 0.3 - 0.8 % |
Titanio | 0.1 - 0.35 % Show Material materials with Titanio of 0.1 - 0.35 % |
Wolframio | 1 - 1.75 % Show Material materials with Wolframio of 1 - 1.75 % |