Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 311 - 388 [-] Show Material materials with Dureza Brinell of 311 - 388 [-] |
Dureza Rockwell C | 23.0 °C | 32 - 41 [-] Show Material materials with Dureza Rockwell C of 32 - 41 [-] |
Elongación A50 | 23.0 °C | 12 % Show Material materials with Elongación A50 of 12 % |
Estricción | 23.0 °C | 15 % Show Material materials with Estricción of 15 % |
Límite elástico Rp 0,2 | 23.0 °C | 830 MPa Show Material materials with Límite elástico Rp 0,2 of 830 MPa |
Resistencia a la tracción | 23.0 °C | 1170 MPa Show Material materials with Resistencia a la tracción of 1170 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.25 % Show Material materials with Aluminio of 0.25 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Boro | 0.01 - 0.07 % Show Material materials with Boro of 0.01 - 0.07 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Cromo | 12 - 15 % Show Material materials with Cromo of 12 - 15 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.25 - 2 % Show Material materials with Manganeso of 1.25 - 2 % |
Molibdeno | 1.25 - 2.25 % Show Material materials with Molibdeno of 1.25 - 2.25 % |
Níquel | 24 - 28 % Show Material materials with Níquel of 24 - 28 % |
Silicona | 0.1 - 0.8 % Show Material materials with Silicona of 0.1 - 0.8 % |
Titanio | 2.7 - 3.3 % Show Material materials with Titanio of 2.7 - 3.3 % |