Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 23 % Show Material materials with Elongación A50 of 23 % |
Elongation A200 | 23.0 °C | 19 % Show Material materials with Elongation A200 of 19 % |
Límite elástico | 23.0 °C | 255 MPa Show Material materials with Límite elástico of 255 MPa |
Resistencia a la tracción | 23.0 °C | 450 - 585 MPa Show Material materials with Resistencia a la tracción of 450 - 585 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.8 % Show Material materials with Azufre of 0.8 % |
Carbono | 0.17 % Show Material materials with Carbono of 0.17 % |
Fósforo | 0.7 % Show Material materials with Fósforo of 0.7 % |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % |
Níquel | 2.1 - 2.5 % Show Material materials with Níquel of 2.1 - 2.5 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |