Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Límite elástico | 275 MPa Show Material materials with Límite elástico of 275 MPa | Normalized | ASTM A203 | Plate |
Resistencia a la tracción | 485 - 620 MPa Show Material materials with Resistencia a la tracción of 485 - 620 MPa | Normalized | ASTM A203 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.8 % Show Material materials with Azufre of 0.8 % | Normalized | ASTM A203 | Plate |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | Normalized | ASTM A203 | Plate |
Fósforo | 0.7 % Show Material materials with Fósforo of 0.7 % | Normalized | ASTM A203 | Plate |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % | Normalized | ASTM A203 | Plate |
Níquel | 3.25 - 3.75 % Show Material materials with Níquel of 3.25 - 3.75 % | Normalized | ASTM A203 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | Normalized | ASTM A203 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |