Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Resistencia a la tracción | 450 - 585 MPa Show Material materials with Resistencia a la tracción of 450 - 585 MPa | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Carbono | 0.18 % Show Material materials with Carbono of 0.18 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Manganeso | 0.9 % Show Material materials with Manganeso of 0.9 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | As-Rolled or Normalized or Normalized and Tempered, or Stress Relieved | ASTM A204 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |