Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Límite elástico | 345 MPa Show Material materials with Límite elástico of 345 MPa | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Resistencia a la tracción | 550 - 690 MPa Show Material materials with Resistencia a la tracción of 550 - 690 MPa | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Manganeso | 1.15 - 1.5 % Show Material materials with Manganeso of 1.15 - 1.5 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Níquel | 0.7 - 1 % Show Material materials with Níquel of 0.7 - 1 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | As-Rolled or Normalized or Normalized and Tempered | ASTM A302 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |