Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Estricción | 45 % Show Material materials with Estricción of 45 % | Quenched and Tempered | ASTM A517 | Plate |
Límite elástico | 620 MPa Show Material materials with Límite elástico of 620 MPa | Quenched and Tempered | ASTM A517 | Plate |
690 MPa Show Material materials with Límite elástico of 690 MPa | Quenched and Tempered | ASTM A517 | Plate | |
Resistencia a la tracción | 725 - 930 MPa Show Material materials with Resistencia a la tracción of 725 - 930 MPa | Quenched and Tempered | ASTM A517 | Plate |
795 - 930 MPa Show Material materials with Resistencia a la tracción of 795 - 930 MPa | Quenched and Tempered | ASTM A517 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Quenched and Tempered | ASTM A517 | Plate |
Boro | 0.0005 - 0.005 % Show Material materials with Boro of 0.0005 - 0.005 % | Quenched and Tempered | ASTM A517 | Plate |
Carbono | 0.15 - 0.21 % Show Material materials with Carbono of 0.15 - 0.21 % | Quenched and Tempered | ASTM A517 | Plate |
Cromo | 0.4 - 0.65 % Show Material materials with Cromo of 0.4 - 0.65 % | Quenched and Tempered | ASTM A517 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Quenched and Tempered | ASTM A517 | Plate |
Manganeso | 0.7 - 1 % Show Material materials with Manganeso of 0.7 - 1 % | Quenched and Tempered | ASTM A517 | Plate |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % | Quenched and Tempered | ASTM A517 | Plate |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % | Quenched and Tempered | ASTM A517 | Plate |
Titanio | 0.01 - 0.04 % Show Material materials with Titanio of 0.01 - 0.04 % | Quenched and Tempered | ASTM A517 | Plate |
Vanadio | 0.03 - 0.08 % Show Material materials with Vanadio of 0.03 - 0.08 % | Quenched and Tempered | ASTM A517 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |