General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | |||
Elongación | 12.6 % Show Material materials with Elongación of 12.6 % | Predicted Value, A200 | |||
14 % Show Material materials with Elongación of 14 % | Quenched and Tempered | ASTM A517 | Plate | A50 | |
14.4 % Show Material materials with Elongación of 14.4 % | Predicted Value, A80 | ||||
16 % Show Material materials with Elongación of 16 % | Quenched and Tempered | ASTM A517 | Plate | A50 | |
18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, Transverse | ||||
19.1 % Show Material materials with Elongación of 19.1 % | Predicted Value | ||||
19.4 % Show Material materials with Elongación of 19.4 % | Predicted Value, A80 Transverse | ||||
Estricción | 42.5 % Show Material materials with Estricción of 42.5 % | Predicted Value, Transverse | |||
45 % Show Material materials with Estricción of 45 % | Quenched and Tempered | ASTM A517 | Plate | ||
Límite elástico | 315.5 MPa Show Material materials with Límite elástico of 315.5 MPa | Predicted Value, RP1 | |||
328.3 MPa Show Material materials with Límite elástico of 328.3 MPa | Predicted Value, RP1 Transverse | ||||
405 MPa Show Material materials with Límite elástico of 405 MPa | Predicted Value, RP05 | ||||
467.9 MPa Show Material materials with Límite elástico of 467.9 MPa | Predicted Value, RP02 Transverse | ||||
497.1 MPa Show Material materials with Límite elástico of 497.1 MPa | Predicted Value, Transverse | ||||
606.1 MPa Show Material materials with Límite elástico of 606.1 MPa | Predicted Value, RP02 | ||||
620 MPa Show Material materials with Límite elástico of 620 MPa | Quenched and Tempered | ASTM A517 | Plate | ||
690 MPa Show Material materials with Límite elástico of 690 MPa | Quenched and Tempered | ASTM A517 | Plate | ||
740.1 MPa Show Material materials with Límite elástico of 740.1 MPa | Predicted Value, RP002 | ||||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | |||
Resistencia a la tracción | 725 - 930 MPa Show Material materials with Resistencia a la tracción of 725 - 930 MPa | Quenched and Tempered | ASTM A517 | Plate | |
795 - 930 MPa Show Material materials with Resistencia a la tracción of 795 - 930 MPa | Quenched and Tempered | ASTM A517 | Plate | ||
Resistencia al cizallamiento | 646.7 MPa Show Material materials with Resistencia al cizallamiento of 646.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 361.5 °C Show Material materials with Temperatura máx. de funcionamiento of 361.5 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 3 S/m Show Material materials with Conductividad eléctrica of 3 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Quenched and Tempered | ASTM A517 | Plate |
Boro | 0.0005 - 0.006 % Show Material materials with Boro of 0.0005 - 0.006 % | Quenched and Tempered | ASTM A517 | Plate |
Carbono | 0.1 - 0.2 % Show Material materials with Carbono of 0.1 - 0.2 % | Quenched and Tempered | ASTM A517 | Plate |
Cobre | 0.15 - 0.5 % Show Material materials with Cobre of 0.15 - 0.5 % | Quenched and Tempered | ASTM A517 | Plate |
Cromo | 0.4 - 0.65 % Show Material materials with Cromo of 0.4 - 0.65 % | Quenched and Tempered | ASTM A517 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Quenched and Tempered | ASTM A517 | Plate |
Manganeso | 0.6 - 1 % Show Material materials with Manganeso of 0.6 - 1 % | Quenched and Tempered | ASTM A517 | Plate |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % | Quenched and Tempered | ASTM A517 | Plate |
Níquel | 0.7 - 1 % Show Material materials with Níquel of 0.7 - 1 % | Quenched and Tempered | ASTM A517 | Plate |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % | Quenched and Tempered | ASTM A517 | Plate |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | Quenched and Tempered | ASTM A517 | Plate |
Vanadio | 0.03 - 0.08 % Show Material materials with Vanadio of 0.03 - 0.08 % | Quenched and Tempered | ASTM A517 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |