General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Chromium Molybdenum Steel |
Elongación A50 | 23.0 °C | 14 - 16 % Show Material materials with Elongación A50 of 14 - 16 % | |
Estricción | 23.0 °C | 45 % Show Material materials with Estricción of 45 % | |
Límite elástico | 23.0 °C | 620 - 690 MPa Show Material materials with Límite elástico of 620 - 690 MPa | |
Módulo de cizallamiento | 23.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Resistencia a la tracción | 23.0 °C | 725 - 930 MPa Show Material materials with Resistencia a la tracción of 725 - 930 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Boro | 5E-4 % Show Material materials with Boro of 5E-4 % |
Carbono | 0.12 - 0.21 % Show Material materials with Carbono of 0.12 - 0.21 % |
Cromo | 0.4 - 0.65 % Show Material materials with Cromo of 0.4 - 0.65 % |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % |
Manganeso | 0.95 - 1.3 % Show Material materials with Manganeso of 0.95 - 1.3 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Níquel | 0.3 - 0.7 % Show Material materials with Níquel of 0.3 - 0.7 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |
Vanadio | 0.03 - 0.08 % Show Material materials with Vanadio of 0.03 - 0.08 % |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |