General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Elongación A50 | 23.0 °C | 14 - 16 % Show Material materials with Elongación A50 of 14 - 16 % | |
Estricción | 23.0 °C | 45 % Show Material materials with Estricción of 45 % | |
Límite elástico | 23.0 °C | 620 - 690 MPa Show Material materials with Límite elástico of 620 - 690 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Resistencia a la tracción | 23.0 °C | 725 - 930 MPa Show Material materials with Resistencia a la tracción of 725 - 930 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Calor específico of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.3E-5 1/K | Typical for Nickel Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 34 - 54 W/(m·K) Show Material materials with Conductividad térmica of 34 - 54 W/(m·K) | Typical for Nickel Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.14 - 0.21 % Show Material materials with Carbono of 0.14 - 0.21 % |
Cromo | 1 - 1.5 % Show Material materials with Cromo of 1 - 1.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.95 - 1.3 % Show Material materials with Manganeso of 0.95 - 1.3 % |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % |
Níquel | 1.2 - 1.5 % Show Material materials with Níquel of 1.2 - 1.5 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |
Vanadio | 0.03 - 0.08 % Show Material materials with Vanadio of 0.03 - 0.08 % |