General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Elongación | 11.5 % Show Material materials with Elongación of 11.5 % | Predicted Value, A200 | |||
13 % Show Material materials with Elongación of 13 % | Quenched and Tempered | ASTM A542 | Plate | A50 | |
16.0 % Show Material materials with Elongación of 16.0 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Elongación of 18.4 % | Predicted Value, Transverse | ||||
19.4 % Show Material materials with Elongación of 19.4 % | Predicted Value | ||||
20.2 % Show Material materials with Elongación of 20.2 % | Predicted Value, A80 Transverse | ||||
Estricción | 41.1 % Show Material materials with Estricción of 41.1 % | Predicted Value | |||
45.1 % Show Material materials with Estricción of 45.1 % | Predicted Value, Transverse | ||||
Límite elástico | 310.9 MPa Show Material materials with Límite elástico of 310.9 MPa | Predicted Value, RP1 | |||
330.2 MPa Show Material materials with Límite elástico of 330.2 MPa | Predicted Value, RP1 Transverse | ||||
363.4 MPa Show Material materials with Límite elástico of 363.4 MPa | Predicted Value, RP05 | ||||
491.6 MPa Show Material materials with Límite elástico of 491.6 MPa | Predicted Value, RP02 Transverse | ||||
516.2 MPa Show Material materials with Límite elástico of 516.2 MPa | Predicted Value, Transverse | ||||
657.2 MPa Show Material materials with Límite elástico of 657.2 MPa | Predicted Value, RP02 | ||||
690 MPa Show Material materials with Límite elástico of 690 MPa | Quenched and Tempered | ASTM A542 | Plate | ||
768 MPa Show Material materials with Límite elástico of 768 MPa | Predicted Value, RP002 | ||||
Módulo de cizallamiento | 80 GPa Show Material materials with Módulo de cizallamiento of 80 GPa | Predicted Value | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Resistencia a la tracción | 795 - 930 MPa Show Material materials with Resistencia a la tracción of 795 - 930 MPa | Quenched and Tempered | ASTM A542 | Plate | |
Resistencia al cizallamiento | 616.7 MPa Show Material materials with Resistencia al cizallamiento of 616.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 1.1e-05 - 1.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % | Quenched and Tempered | ASTM A542 | Plate |
Cobre | 0.4 % Show Material materials with Cobre of 0.4 % | Quenched and Tempered | ASTM A542 | Plate |
Cromo | 2 - 2.5 % Show Material materials with Cromo of 2 - 2.5 % | Quenched and Tempered | ASTM A542 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Quenched and Tempered | ASTM A542 | Plate |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % | Quenched and Tempered | ASTM A542 | Plate |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % | Quenched and Tempered | ASTM A542 | Plate |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % | Quenched and Tempered | ASTM A542 | Plate |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | Quenched and Tempered | ASTM A542 | Plate |
Vanadio | 0.03 % Show Material materials with Vanadio of 0.03 % | Quenched and Tempered | ASTM A542 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |