Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % |
Energía de impacto Charpy | 23.0 °C | 27 - 34 J Show Material materials with Energía de impacto Charpy of 27 - 34 J |
Límite elástico Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa |
Resistencia a la tracción | 23.0 °C | 655 - 795 MPa Show Material materials with Resistencia a la tracción of 655 - 795 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 - 0.12 % Show Material materials with Aluminio of 0.02 - 0.12 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.13 % Show Material materials with Carbono of 0.13 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % |
Molibdeno | 0.2 - 0.35 % Show Material materials with Molibdeno of 0.2 - 0.35 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 4.8 - 5.2 % Show Material materials with Níquel of 4.8 - 5.2 % |
Silicona | 0.2 - 0.4 % Show Material materials with Silicona of 0.2 - 0.4 % |