Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Energía de impacto Charpy | 27 J Show Material materials with Energía de impacto Charpy of 27 J | Heat-Treated | ASTM A738 | Plate |
Límite elástico | 315 MPa Show Material materials with Límite elástico of 315 MPa | Heat-Treated | ASTM A738 | Plate |
380 MPa Show Material materials with Límite elástico of 380 MPa | Heat-Treated | ASTM A738 | Plate | |
415 MPa Show Material materials with Límite elástico of 415 MPa | Heat-Treated | ASTM A738 | Plate | |
Resistencia a la tracción | 485 - 620 MPa Show Material materials with Resistencia a la tracción of 485 - 620 MPa | Heat-Treated | ASTM A738 | Plate |
515 - 655 MPa Show Material materials with Resistencia a la tracción of 515 - 655 MPa | Heat-Treated | ASTM A738 | Plate | |
550 - 690 MPa Show Material materials with Resistencia a la tracción of 550 - 690 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | Heat-Treated | ASTM A738 | Plate |
Cobre | 0.35 % Show Material materials with Cobre of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | Heat-Treated | ASTM A738 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Heat-Treated | ASTM A738 | Plate |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % | Heat-Treated | ASTM A738 | Plate |
Molibdeno | 0.08 % Show Material materials with Molibdeno of 0.08 % | Heat-Treated | ASTM A738 | Plate |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % | Heat-Treated | ASTM A738 | Plate |
Silicona | 0.15 - 0.5 % Show Material materials with Silicona of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |