Mecánica
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Energía de impacto Charpy | 27 J Show Material materials with Energía de impacto Charpy of 27 J | Heat-Treated | ASTM A738 | Plate |
Límite elástico | 515 MPa Show Material materials with Límite elástico of 515 MPa | Heat-Treated | ASTM A738 | Plate |
Resistencia a la tracción | 620 - 760 MPa Show Material materials with Resistencia a la tracción of 620 - 760 MPa | Heat-Treated | ASTM A738 | Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | Heat-Treated | ASTM A738 | Plate |
Azufre | 0.006 % Show Material materials with Azufre of 0.006 % | Heat-Treated | ASTM A738 | Plate |
Boro | 0.0007 % Show Material materials with Boro of 0.0007 % | Heat-Treated | ASTM A738 | Plate |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % | Heat-Treated | ASTM A738 | Plate |
Cobre | 0.35 % Show Material materials with Cobre of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | Heat-Treated | ASTM A738 | Plate |
Fósforo | 0.015 % Show Material materials with Fósforo of 0.015 % | Heat-Treated | ASTM A738 | Plate |
Manganeso | 1.1 - 1.6 % Show Material materials with Manganeso of 1.1 - 1.6 % | Heat-Treated | ASTM A738 | Plate |
Molibdeno | 0.35 % Show Material materials with Molibdeno of 0.35 % | Heat-Treated | ASTM A738 | Plate |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % | Heat-Treated | ASTM A738 | Plate |
Níquel | 0.7 % Show Material materials with Níquel of 0.7 % | Heat-Treated | ASTM A738 | Plate |
Silicona | 0.15 - 0.5 % Show Material materials with Silicona of 0.15 - 0.5 % | Heat-Treated | ASTM A738 | Plate |
Vanadio | 0.09 % Show Material materials with Vanadio of 0.09 % | Heat-Treated | ASTM A738 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |