General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 244 [-] Show Material materials with Dureza Brinell of 244 [-] | Predicted Value, Transverse |
Elongación | 14.2 % Show Material materials with Elongación of 14.2 % | Predicted Value, A200 |
15.6 % Show Material materials with Elongación of 15.6 % | Predicted Value, A80 | |
18.3 % Show Material materials with Elongación of 18.3 % | Predicted Value, Transverse | |
19.6 % Show Material materials with Elongación of 19.6 % | Predicted Value, A80 Transverse | |
20.3 % Show Material materials with Elongación of 20.3 % | Predicted Value, A5 | |
21.2 % Show Material materials with Elongación of 21.2 % | Predicted Value, A50 | |
21.4 % Show Material materials with Elongación of 21.4 % | Predicted Value | |
Estricción | 41.6 % Show Material materials with Estricción of 41.6 % | Predicted Value |
43.1 % Show Material materials with Estricción of 43.1 % | Predicted Value, Transverse | |
Módulo de cizallamiento | 79.5 GPa Show Material materials with Módulo de cizallamiento of 79.5 GPa | Predicted Value |
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia al cizallamiento | 515.9 MPa Show Material materials with Resistencia al cizallamiento of 515.9 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 460.9 J/(kg·K) Show Material materials with Calor específico of 460.9 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.78 1/K Show Material materials with Coeficiente de dilatación térmica of 11.78 1/K | Predicted Value |
Conductividad térmica | 40.51 W/(m·K) Show Material materials with Conductividad térmica of 40.51 W/(m·K) | Predicted Value |
Temperatura máx. de funcionamiento | 299.5 °C Show Material materials with Temperatura máx. de funcionamiento of 299.5 °C | Predicted Value, Long |
Eléctrico
Chemical properties
Property | Value | Related Standards |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | ASTM A572 |
Carbono | 0.23 % Show Material materials with Carbono of 0.23 % | ASTM A572 |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | ASTM A572 |
Manganeso | 1.65 % Show Material materials with Manganeso of 1.65 % | ASTM A572 |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | ASTM A572 |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |