General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 25 - 28 % Show Material materials with Elongación A50 of 25 - 28 % | |
Energía de impacto Charpy | 23.0 °C | 95 J Show Material materials with Energía de impacto Charpy of 95 J | |
Estricción | 23.0 °C | 60 % Show Material materials with Estricción of 60 % | |
Límite elástico Rp 0,2 | 23.0 °C | 760 - 930 MPa Show Material materials with Límite elástico Rp 0,2 of 760 - 930 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 830 - 1000 MPa Show Material materials with Resistencia a la tracción of 830 - 1000 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.04 % Show Material materials with Aluminio of 0.04 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 17.5 - 20 % Show Material materials with Cromo of 17.5 - 20 % |
Fósforo | 0.06 % Show Material materials with Fósforo of 0.06 % |
Manganeso | 17.5 - 20 % Show Material materials with Manganeso of 17.5 - 20 % |
Nitrógeno | 0.45 - 0.8 % Show Material materials with Nitrógeno of 0.45 - 0.8 % |
Níquel | 2 % Show Material materials with Níquel of 2 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |
Vanadio | 0.25 % Show Material materials with Vanadio of 0.25 % |