General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Steel |
Dureza Brinell | 20.0 °C | 207 [-] Show Material materials with Dureza Brinell of 207 [-] | |
Dureza Rockwell B | 20.0 °C | 92 [-] Show Material materials with Dureza Rockwell B of 92 [-] | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 440 - 494 J/(kg·K) Show Material materials with Calor específico of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Coeficiente de dilatación térmica | 20.0 °C | 9.4E-6 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
Conductividad térmica | 20.0 °C | 23 - 50 W/(m·K) Show Material materials with Conductividad térmica of 23 - 50 W/(m·K) | Typical for Chromium Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.93 - 1.05 % Show Material materials with Carbono of 0.93 - 1.05 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 1.35 - 1.6 % Show Material materials with Cromo of 1.35 - 1.6 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.25 - 0.45 % Show Material materials with Manganeso of 0.25 - 0.45 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Oxígeno | 1.5E-3 % Show Material materials with Oxígeno of 1.5E-3 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |