General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for High Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for High Carbon Steel |
Dureza Brinell | 20.0 °C | 331 [-] Show Material materials with Dureza Brinell of 331 [-] | |
Módulo de cizallamiento | 20.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for High Carbon Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | Typical for High Carbon Steel |
Temperatura de fusión | 1289 - 1478 °C Show Material materials with Temperatura de fusión of 1289 - 1478 °C | Typical for High Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.65 - 0.75 % Show Material materials with Carbono of 0.65 - 0.75 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.2 % Show Material materials with Cromo of 0.2 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.8 - 1.1 % Show Material materials with Manganeso of 0.8 - 1.1 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Oxígeno | 1.5E-3 % Show Material materials with Oxígeno of 1.5E-3 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |