General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Límite elástico | 23.0 °C | 415 MPa Show Material materials with Límite elástico of 415 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 620 - 760 MPa Show Material materials with Resistencia a la tracción of 620 - 760 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1370 - 1530 °C Show Material materials with Temperatura de fusión of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Antimonio | 3E-3 % Show Material materials with Antimonio of 3E-3 % |
Arsénico | 0.01 % Show Material materials with Arsénico of 0.01 % |
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Boro | 1E-3 % Show Material materials with Boro of 1E-3 % |
Carbono | 0.08 - 0.12 % Show Material materials with Carbono of 0.08 - 0.12 % |
Circonio | 0.01 % Show Material materials with Circonio of 0.01 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Cromo | 8 - 9.5 % Show Material materials with Cromo of 8 - 9.5 % |
Estaño | 0.01 % Show Material materials with Estaño of 0.01 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.3 - 0.5 % Show Material materials with Manganeso of 0.3 - 0.5 % |
Molibdeno | 0.85 - 1.05 % Show Material materials with Molibdeno of 0.85 - 1.05 % |
Niobio | 0.06 - 0.1 % Show Material materials with Niobio of 0.06 - 0.1 % |
Nitrógeno | 0.04 - 0.07 % Show Material materials with Nitrógeno of 0.04 - 0.07 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Silicona | 0.2 - 0.4 % Show Material materials with Silicona of 0.2 - 0.4 % |
Titanio | 0.01 % Show Material materials with Titanio of 0.01 % |
Vanadio | 0.18 - 0.25 % Show Material materials with Vanadio of 0.18 - 0.25 % |
Wolframio | 0.05 % Show Material materials with Wolframio of 0.05 % |