General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 223 - 269 [-] Show Material materials with Dureza Brinell of 223 - 269 [-] | |
Dureza Rockwell B | 23.0 °C | 98 - 104 [-] Show Material materials with Dureza Rockwell B of 98 - 104 [-] | |
Dureza Rockwell C | 23.0 °C | 19 - 28 [-] Show Material materials with Dureza Rockwell C of 19 - 28 [-] | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.95 - 1.3 % Show Material materials with Aluminio of 0.95 - 1.3 % |
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.22 - 0.27 % Show Material materials with Carbono of 0.22 - 0.27 % |
Cromo | 1 - 1.35 % Show Material materials with Cromo of 1 - 1.35 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 0.7 % Show Material materials with Manganeso of 0.5 - 0.7 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Níquel | 3.25 - 3.75 % Show Material materials with Níquel of 3.25 - 3.75 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |