General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Energía de impacto Charpy | 23.0 °C | 16 J Show Material materials with Energía de impacto Charpy of 16 J | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Límite elástico | 23.0 °C | 485 MPa Show Material materials with Límite elástico of 485 MPa | |
Límite elástico Rp 0,2 | 23.0 °C | 520 MPa Show Material materials with Límite elástico Rp 0,2 of 520 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 655 MPa Show Material materials with Resistencia a la tracción of 655 MPa | |
Yield strength Rp0.02 | 23.0 °C | 485 MPa Show Material materials with Yield strength Rp0.02 of 485 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.015 % Show Material materials with Aluminio of 0.015 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Cromo | 0.75 % Show Material materials with Cromo of 0.75 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % |
Molibdeno | 0.25 % Show Material materials with Molibdeno of 0.25 % |
Níquel | 2 % Show Material materials with Níquel of 2 % |
Vanadio | 0.03 - 0.12 % Show Material materials with Vanadio of 0.03 - 0.12 % |