General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Densidad of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Estricción | 23.0 °C | 38 % Show Material materials with Estricción of 38 % | |
Límite elástico Rp 0,2 | 23.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 485 - 655 MPa Show Material materials with Resistencia a la tracción of 485 - 655 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.03 % Show Material materials with Aluminio of 0.03 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Boro | 3E-3 % Show Material materials with Boro of 3E-3 % |
Calcio | 0.02 % Show Material materials with Calcio of 0.02 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.7 - 1.35 % Show Material materials with Manganeso of 0.7 - 1.35 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Niobio | 0.01 % Show Material materials with Niobio of 0.01 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |