Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 18 % Show Material materials with Elongación A50 of 18 % |
Estricción | 20.0 °C | 38 % Show Material materials with Estricción of 38 % |
Resistencia a la tracción | 20.0 °C | 550 - 725 MPa Show Material materials with Resistencia a la tracción of 550 - 725 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 345 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 345 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.03 % Show Material materials with Aluminio of 0.03 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Boro | 3E-3 % Show Material materials with Boro of 3E-3 % |
Calcio | 0.02 % Show Material materials with Calcio of 0.02 % |
Carbono | 0.27 % Show Material materials with Carbono of 0.27 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 0.25 - 0.45 % Show Material materials with Cromo of 0.25 - 0.45 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 1 % Show Material materials with Manganeso of 0.5 - 1 % |
Molibdeno | 0.55 - 0.7 % Show Material materials with Molibdeno of 0.55 - 0.7 % |
Niobio | 0.01 % Show Material materials with Niobio of 0.01 % |
Níquel | 0.5 - 1 % Show Material materials with Níquel of 0.5 - 1 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |