General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Estricción | 23.0 °C | 48 % Show Material materials with Estricción of 48 % | |
Límite elástico Rp 0,2 | 23.0 °C | 485 MPa Show Material materials with Límite elástico Rp 0,2 of 485 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 620 - 795 MPa Show Material materials with Resistencia a la tracción of 620 - 795 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.025 % Show Material materials with Aluminio of 0.025 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Boro | 3E-3 % Show Material materials with Boro of 3E-3 % |
Calcio | 0.02 % Show Material materials with Calcio of 0.02 % |
Carbono | 0.23 % Show Material materials with Carbono of 0.23 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Cromo | 1.5 - 2 % Show Material materials with Cromo of 1.5 - 2 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % |
Niobio | 0.01 % Show Material materials with Niobio of 0.01 % |
Níquel | 2.8 - 3.9 % Show Material materials with Níquel of 2.8 - 3.9 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % |
Vanadio | 0.03 % Show Material materials with Vanadio of 0.03 % |