Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 20 % Show Material materials with Elongación A50 of 20 % |
Estricción | 20.0 °C | 48 % Show Material materials with Estricción of 48 % |
Resistencia a la tracción | 20.0 °C | 620 - 795 MPa Show Material materials with Resistencia a la tracción of 620 - 795 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 485 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 485 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.03 % Show Material materials with Aluminio of 0.03 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 3E-3 % Show Material materials with Boro of 3E-3 % |
Calcio | 0.02 % Show Material materials with Calcio of 0.02 % |
Carbono | 0.11 - 0.15 % Show Material materials with Carbono of 0.11 - 0.15 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Cromo | 2 - 2.5 % Show Material materials with Cromo of 2 - 2.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % |
Niobio | 0.01 % Show Material materials with Niobio of 0.01 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % |
Vanadio | 0.02 % Show Material materials with Vanadio of 0.02 % |