Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % |
Energía de impacto Charpy | 23.0 °C | 20 J Show Material materials with Energía de impacto Charpy of 20 J |
Estricción | 23.0 °C | 38 % Show Material materials with Estricción of 38 % |
Límite elástico Rp 0,2 | 23.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa |
Resistencia a la tracción | 23.0 °C | 485 - 655 MPa Show Material materials with Resistencia a la tracción of 485 - 655 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.35 % Show Material materials with Carbono of 0.35 % |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 0.9 % Show Material materials with Manganeso of 0.4 - 0.9 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |