General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % | |
Energía de impacto Charpy | 20.0 °C | 60 J Show Material materials with Energía de impacto Charpy of 60 J | |
Estricción | 20.0 °C | 36 % Show Material materials with Estricción of 36 % | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 1210 MPa Show Material materials with Resistencia a la tracción of 1210 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Conductividad térmica | 20.0 °C | 44 W/(m·K) Show Material materials with Conductividad térmica of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.23 - 0.28 % Show Material materials with Carbono of 0.23 - 0.28 % |
Cromo | 1.4 - 1.65 % Show Material materials with Cromo of 1.4 - 1.65 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Molibdeno | 0.8 - 1 % Show Material materials with Molibdeno of 0.8 - 1 % |
Níquel | 2.75 - 3.25 % Show Material materials with Níquel of 2.75 - 3.25 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |