Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 9 - 13 % Show Material materials with Elongación of 9 - 13 % |
Energía de impacto Charpy | 20.0 °C | 15 - 25 J Show Material materials with Energía de impacto Charpy of 15 - 25 J |
Estricción | 20.0 °C | 28 - 40 % Show Material materials with Estricción of 28 - 40 % |
Resistencia a la tracción | 20.0 °C | 1035 - 1450 MPa Show Material materials with Resistencia a la tracción of 1035 - 1450 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1380 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1380 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.27 - 0.33 % Show Material materials with Carbono of 0.27 - 0.33 % |
Cromo | 0.8 - 1.1 % Show Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 0.6 % Show Material materials with Manganeso of 0.4 - 0.6 % |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % |
Silicona | 0.2 - 0.35 % Show Material materials with Silicona of 0.2 - 0.35 % |
Vanadio | 0.05 - 0.1 % Show Material materials with Vanadio of 0.05 - 0.1 % |