Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 6 - 13 % Show Material materials with Elongación of 6 - 13 % |
Energía de impacto Charpy | 20.0 °C | 15 - 45 J Show Material materials with Energía de impacto Charpy of 15 - 45 J |
Estricción | 20.0 °C | 25 - 40 % Show Material materials with Estricción of 25 - 40 % |
Resistencia a la tracción | 20.0 °C | 1035 - 1720 MPa Show Material materials with Resistencia a la tracción of 1035 - 1720 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1550 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.45 - 0.5 % Show Material materials with Carbono of 0.45 - 0.5 % |
Cromo | 0.9 - 1.2 % Show Material materials with Cromo of 0.9 - 1.2 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.6 - 0.9 % Show Material materials with Manganeso of 0.6 - 0.9 % |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % |
Níquel | 0.4 - 0.7 % Show Material materials with Níquel of 0.4 - 0.7 % |
Silicona | 0.15 - 0.3 % Show Material materials with Silicona of 0.15 - 0.3 % |
Vanadio | 0.08 - 0.15 % Show Material materials with Vanadio of 0.08 - 0.15 % |