Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 6 % Show Material materials with Elongación of 6 % |
Energía de impacto Charpy | 20.0 °C | 20 J Show Material materials with Energía de impacto Charpy of 20 J |
Estricción | 20.0 °C | 25 % Show Material materials with Estricción of 25 % |
Resistencia a la tracción | 20.0 °C | 1720 MPa Show Material materials with Resistencia a la tracción of 1720 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1550 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.41 - 0.46 % Show Material materials with Carbono of 0.41 - 0.46 % |
Cromo | 1.9 - 2.25 % Show Material materials with Cromo of 1.9 - 2.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.75 - 1 % Show Material materials with Manganeso of 0.75 - 1 % |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % |
Silicona | 1.4 - 1.75 % Show Material materials with Silicona of 1.4 - 1.75 % |
Vanadio | 0.03 - 0.08 % Show Material materials with Vanadio of 0.03 - 0.08 % |