Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 8 - 9 % Show Material materials with Elongación of 8 - 9 % |
Energía de impacto Charpy | 20.0 °C | 20 J Show Material materials with Energía de impacto Charpy of 20 J |
Estricción | 20.0 °C | 25 - 30 % Show Material materials with Estricción of 25 - 30 % |
Resistencia a la tracción | 20.0 °C | 1790 - 1930 MPa Show Material materials with Resistencia a la tracción of 1790 - 1930 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1380 - 1550 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1380 - 1550 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.38 - 0.43 % Show Material materials with Carbono of 0.38 - 0.43 % |
Cromo | 4.75 - 5.25 % Show Material materials with Cromo of 4.75 - 5.25 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % |
Molibdeno | 1.2 - 1.4 % Show Material materials with Molibdeno of 1.2 - 1.4 % |
Silicona | 0.8 - 1 % Show Material materials with Silicona of 0.8 - 1 % |
Vanadio | 0.4 - 0.6 % Show Material materials with Vanadio of 0.4 - 0.6 % |