Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Elongación | 20.0 °C | 10 - 12 % Show Material materials with Elongación of 10 - 12 % | |
Estricción | 20.0 °C | 40 - 45 % Show Material materials with Estricción of 40 - 45 % | |
Módulo elástico | 20.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 1210 - 1520 MPa Show Material materials with Resistencia a la tracción of 1210 - 1520 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.2 - 0.25 % Show Material materials with Carbono of 0.2 - 0.25 % |
Cobalto | 0.25 % Show Material materials with Cobalto of 0.25 % |
Cromo | 11 - 12.5 % Show Material materials with Cromo of 11 - 12.5 % |
Estaño | 0.04 % Show Material materials with Estaño of 0.04 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 1 % Show Material materials with Manganeso of 0.5 - 1 % |
Molibdeno | 0.9 - 1.25 % Show Material materials with Molibdeno of 0.9 - 1.25 % |
Níquel | 0.5 - 1 % Show Material materials with Níquel of 0.5 - 1 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |
Vanadio | 0.2 - 0.3 % Show Material materials with Vanadio of 0.2 - 0.3 % |
Wolframio | 0.9 - 1.25 % Show Material materials with Wolframio of 0.9 - 1.25 % |