Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 8 - 12 % Show Material materials with Elongación of 8 - 12 % |
Energía de impacto Charpy | 20.0 °C | 35 J Show Material materials with Energía de impacto Charpy of 35 J |
Estricción | 20.0 °C | 40 - 50 % Show Material materials with Estricción of 40 - 50 % |
Resistencia a la tracción | 20.0 °C | 1140 - 1380 MPa Show Material materials with Resistencia a la tracción of 1140 - 1380 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1240 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cobre | 3 - 5 % Show Material materials with Cobre of 3 - 5 % |
Cromo | 15.5 - 17.5 % Show Material materials with Cromo of 15.5 - 17.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Niobio | 0.15 - 0.45 % Show Material materials with Niobio of 0.15 - 0.45 % |
Níquel | 3 - 5 % Show Material materials with Níquel of 3 - 5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |