Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 6 % Show Material materials with Elongación of 6 % |
Estricción | 20.0 °C | 25 % Show Material materials with Estricción of 25 % |
Resistencia a la tracción | 20.0 °C | 1140 - 1240 MPa Show Material materials with Resistencia a la tracción of 1140 - 1240 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1100 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1100 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.75 - 1.5 % Show Material materials with Aluminio of 0.75 - 1.5 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.09 % Show Material materials with Carbono of 0.09 % |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 6.5 - 7.75 % Show Material materials with Níquel of 6.5 - 7.75 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |