Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 5 - 6 % Show Material materials with Elongación of 5 - 6 % |
Estricción | 20.0 °C | 25 % Show Material materials with Estricción of 25 % |
Resistencia a la tracción | 20.0 °C | 1240 - 1550 MPa Show Material materials with Resistencia a la tracción of 1240 - 1550 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1100 - 1380 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1100 - 1380 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.75 - 1.25 % Show Material materials with Aluminio of 0.75 - 1.25 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.09 % Show Material materials with Carbono of 0.09 % |
Cromo | 14 - 15.25 % Show Material materials with Cromo of 14 - 15.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 2 - 2.75 % Show Material materials with Molibdeno of 2 - 2.75 % |
Níquel | 6.5 - 7.75 % Show Material materials with Níquel of 6.5 - 7.75 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |