Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 10 - 12 % Show Material materials with Elongación of 10 - 12 % |
Energía de impacto Charpy | 20.0 °C | 20 J Show Material materials with Energía de impacto Charpy of 20 J |
Estricción | 20.0 °C | 25 % Show Material materials with Estricción of 25 % |
Resistencia a la tracción | 20.0 °C | 1140 - 1450 MPa Show Material materials with Resistencia a la tracción of 1140 - 1450 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 965 - 1240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 965 - 1240 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.1 - 0.15 % Show Material materials with Carbono of 0.1 - 0.15 % |
Cromo | 15 - 16 % Show Material materials with Cromo of 15 - 16 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 1.25 % Show Material materials with Manganeso of 0.5 - 1.25 % |
Molibdeno | 2.5 - 3.25 % Show Material materials with Molibdeno of 2.5 - 3.25 % |
Nitrógeno | 0.07 - 0.13 % Show Material materials with Nitrógeno of 0.07 - 0.13 % |
Níquel | 4 - 5 % Show Material materials with Níquel of 4 - 5 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |