General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Elongación | 20.0 °C | 10 % Show Material materials with Elongación of 10 % | |
Energía de impacto Charpy | 20.0 °C | 25 J Show Material materials with Energía de impacto Charpy of 25 J | |
Estricción | 20.0 °C | 45 % Show Material materials with Estricción of 45 % | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 1760 MPa Show Material materials with Resistencia a la tracción of 1760 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1720 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1720 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Conductividad térmica | 20.0 °C | 44 W/(m·K) Show Material materials with Conductividad térmica of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 - 0.15 % Show Material materials with Aluminio of 0.05 - 0.15 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobalto | 7 - 8.5 % Show Material materials with Cobalto of 7 - 8.5 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Molibdeno | 4.6 - 5.2 % Show Material materials with Molibdeno of 4.6 - 5.2 % |
Níquel | 17 - 19 % Show Material materials with Níquel of 17 - 19 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Titanio | 0.3 - 0.5 % Show Material materials with Titanio of 0.3 - 0.5 % |