General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Elongación | 20.0 °C | 4 - 7 % Show Material materials with Elongación of 4 - 7 % | |
Energía de impacto Charpy | 20.0 °C | 15 J Show Material materials with Energía de impacto Charpy of 15 J | |
Estricción | 20.0 °C | 15 - 20 % Show Material materials with Estricción of 15 - 20 % | |
Módulo elástico | 20.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 1790 - 1930 MPa Show Material materials with Resistencia a la tracción of 1790 - 1930 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 1550 - 1720 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 1550 - 1720 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 20.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.42 - 0.47 % Show Material materials with Carbono of 0.42 - 0.47 % |
Cobalto | 3.5 - 4.5 % Show Material materials with Cobalto of 3.5 - 4.5 % |
Cromo | 0.2 - 0.35 % Show Material materials with Cromo of 0.2 - 0.35 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.1 - 0.35 % Show Material materials with Manganeso of 0.1 - 0.35 % |
Molibdeno | 0.2 - 0.35 % Show Material materials with Molibdeno of 0.2 - 0.35 % |
Níquel | 7 - 8.5 % Show Material materials with Níquel of 7 - 8.5 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Vanadio | 0.06 - 0.12 % Show Material materials with Vanadio of 0.06 - 0.12 % |