Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 248 [-] Show Material materials with Dureza Brinell of 248 [-] |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % |
Estricción | 23.0 °C | 18 % Show Material materials with Estricción of 18 % |
Límite elástico Rp 0,2 | 23.0 °C | 550 - 585 MPa Show Material materials with Límite elástico Rp 0,2 of 550 - 585 MPa |
Resistencia a la tracción | 23.0 °C | 860 - 895 MPa Show Material materials with Resistencia a la tracción of 860 - 895 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.35 % Show Material materials with Aluminio of 0.35 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Boro | 0.001 - 0.01 % Show Material materials with Boro of 0.001 - 0.01 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 12 - 15 % Show Material materials with Cromo of 12 - 15 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Molibdeno | 2.5 - 3.5 % Show Material materials with Molibdeno of 2.5 - 3.5 % |
Níquel | 24 - 28 % Show Material materials with Níquel of 24 - 28 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 1.55 - 2 % Show Material materials with Titanio of 1.55 - 2 % |