Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.72 - 8 g/cm³ Show Material materials with Densidad of 7.72 - 8 g/cm³ | Typical for Tool And Machining Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Tool And Machining Steel |
Dureza Brinell | 23.0 °C | 255 [-] Show Material materials with Dureza Brinell of 255 [-] | |
Módulo de cizallamiento | 23.0 °C | 79 GPa Show Material materials with Módulo de cizallamiento of 79 GPa | Typical for Tool And Machining Steel |
Módulo elástico | 23.0 °C | 203 - 211 GPa Show Material materials with Módulo elástico of 203 - 211 GPa | Typical for Tool And Machining Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 420 - 460 J/(kg·K) Show Material materials with Calor específico of 420 - 460 J/(kg·K) | Typical for Tool And Machining Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.3E-5 1/K | Typical for Tool And Machining Steel |
Conductividad térmica | 23.0 °C | 17 - 42 W/(m·K) Show Material materials with Conductividad térmica of 17 - 42 W/(m·K) | Typical for Tool And Machining Steel |
Temperatura de fusión | 1370 - 1425 °C Show Material materials with Temperatura de fusión of 1370 - 1425 °C | Typical for Tool And Machining Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.45 - 0.55 % Show Material materials with Carbono of 0.45 - 0.55 % |
Cromo | 3 - 3.5 % Show Material materials with Cromo of 3 - 3.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.2 - 0.9 % Show Material materials with Manganeso of 0.2 - 0.9 % |
Molibdeno | 1.3 - 1.8 % Show Material materials with Molibdeno of 1.3 - 1.8 % |
Silicona | 0.2 - 1 % Show Material materials with Silicona of 0.2 - 1 % |
Vanadio | 0.35 % Show Material materials with Vanadio of 0.35 % |