General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Densidad of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Dureza Brinell | 23.0 °C | 341 [-] Show Material materials with Dureza Brinell of 341 [-] | |
Dureza Rockwell C | 23.0 °C | 37 [-] Show Material materials with Dureza Rockwell C of 37 [-] | |
Elongación A50 | 23.0 °C | 12 % Show Material materials with Elongación A50 of 12 % | |
Estricción | 23.0 °C | 25 % Show Material materials with Estricción of 25 % | |
Límite elástico | 23.0 °C | 1070 MPa Show Material materials with Límite elástico of 1070 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 1170 MPa Show Material materials with Resistencia a la tracción of 1170 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1370 - 1530 °C Show Material materials with Temperatura de fusión of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.1 - 0.15 % Show Material materials with Carbono of 0.1 - 0.15 % |
Cromo | 15 - 16 % Show Material materials with Cromo of 15 - 16 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 1.25 % Show Material materials with Manganeso of 0.5 - 1.25 % |
Molibdeno | 2.5 - 3.25 % Show Material materials with Molibdeno of 2.5 - 3.25 % |
Níquel | 4 - 5 % Show Material materials with Níquel of 4 - 5 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |