General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 331 [-] Show Material materials with Dureza Brinell of 331 [-] | |
Dureza Rockwell C | 23.0 °C | 35 [-] Show Material materials with Dureza Rockwell C of 35 [-] | |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Límite elástico | 23.0 °C | 1035 MPa Show Material materials with Límite elástico of 1035 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1170 MPa Show Material materials with Resistencia a la tracción of 1170 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cromo | 16 - 17.5 % Show Material materials with Cromo of 16 - 17.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 6 - 7.5 % Show Material materials with Níquel of 6 - 7.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.4 - 1.2 % Show Material materials with Titanio of 0.4 - 1.2 % |