General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 430 [-] Show Material materials with Dureza Brinell of 430 [-] | |
Dureza Rockwell C | 23.0 °C | 45 [-] Show Material materials with Dureza Rockwell C of 45 [-] | |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Estricción | 23.0 °C | 35 - 45 % Show Material materials with Estricción of 35 - 45 % | |
Límite elástico | 23.0 °C | 1420 MPa Show Material materials with Límite elástico of 1420 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1520 MPa Show Material materials with Resistencia a la tracción of 1520 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.9 - 1.35 % Show Material materials with Aluminio of 0.9 - 1.35 % |
Azufre | 8E-3 % Show Material materials with Azufre of 8E-3 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cromo | 12.25 - 13.25 % Show Material materials with Cromo of 12.25 - 13.25 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Molibdeno | 2 - 2.5 % Show Material materials with Molibdeno of 2 - 2.5 % |
Níquel | 7.5 - 8.5 % Show Material materials with Níquel of 7.5 - 8.5 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |