General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 415 [-] Show Material materials with Dureza Brinell of 415 [-] | |
Dureza Rockwell C | 23.0 °C | 44 [-] Show Material materials with Dureza Rockwell C of 44 [-] | |
Elongación A50 | 23.0 °C | 5 - 10 % Show Material materials with Elongación A50 of 5 - 10 % | |
Estricción | 23.0 °C | 20 - 40 % Show Material materials with Estricción of 20 - 40 % | |
Límite elástico | 23.0 °C | 1410 MPa Show Material materials with Límite elástico of 1410 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1520 MPa Show Material materials with Resistencia a la tracción of 1520 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobre | 1.5 - 2.5 % Show Material materials with Cobre of 1.5 - 2.5 % |
Cromo | 11 - 12.5 % Show Material materials with Cromo of 11 - 12.5 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 7.5 - 9.5 % Show Material materials with Níquel of 7.5 - 9.5 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |
Titanio | 1 - 1.35 % Show Material materials with Titanio of 1 - 1.35 % |