General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 321 [-] Show Material materials with Dureza Brinell of 321 [-] | |
Dureza Rockwell C | 23.0 °C | 34 [-] Show Material materials with Dureza Rockwell C of 34 [-] | |
Elongación A50 | 23.0 °C | 9 - 12 % Show Material materials with Elongación A50 of 9 - 12 % | |
Estricción | 23.0 °C | 30 - 45 % Show Material materials with Estricción of 30 - 45 % | |
Límite elástico | 23.0 °C | 930 MPa Show Material materials with Límite elástico of 930 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1000 MPa Show Material materials with Resistencia a la tracción of 1000 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobre | 1.25 - 1.75 % Show Material materials with Cobre of 1.25 - 1.75 % |
Cromo | 14 - 16 % Show Material materials with Cromo of 14 - 16 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.5 - 1 % Show Material materials with Molibdeno of 0.5 - 1 % |
Níquel | 5 - 7 % Show Material materials with Níquel of 5 - 7 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |